Principles and mechanisms of flotation

Flotation is based on differences in the physico-chemical surface properties of minerals. These properties are either already existent or they are induced by corresponding reagents.

A flotation system consists of three different phases represented by water, air, and solid particles. The process takes place in flotation cells. In those cells the fine grained solids are maintained in suspension by agitators or impellers. At the same time a continuous stream of air bubbles rises from the bottom to the top of the cell. For mineral separation certain minerals have to attach to the bubbles which take them to the surface. There the bubbles have to form a stable froth that can carry the floated mineral particles until they are removed from the top of the cell.

Before submitting an ore to flotation it has to be ground to floatable grain sizes. In order to defy the laws of gravity with the help of an air bubble a mineral particle must not exceed certain dimensions, which depend on the specific gravity of the mineral. The upper size limit rarely exceeds 500 microns and is usually below 300 microns. Optimum results are generally obtained with particle sizes ranging from 10 to 100 microns. With particles below 10 microns there are phenomena that strongly affect flotation: Extremely fine particles, so called “slimes”, tend to loose their chemical identity in favour of physical forces that become more and more dominant.

The floatability of a mineral mainly depends from its ability to adhere to air bubbles. This ability is controlled by the surface properties of the mineral. Mineral particles that get readily attached to air bubbles are water repellent or hydrophobic, those that do not attach are hydrophilic.

More or less polar minerals such as most sulphides have to be conditioned by chemical reagents, so called collectors, before they can be recovered by flotation. The collectors are added to the pulp in special conditioning tanks. Collectors are complex organic chemicals that usually possess a polar and a non polar end. The polar end is adsorbed to the polar mineral surface leaving the non polar end toward the water. So the conditioned mineral achieves a water repellent characteristic and gets easily picked up by a rising air bubble. There are also non polar collectors that render a mineral hydrophobic by covering its surface with a thin film. The consumption of a xanthate collector per tonne of ore lies between 20 and 200g.

In addition to collectors frothers have to be added to the pulp to create persistent bubbles and to produce a froth stable enough to carry the load of floated minerals at the top of the flotation cell. Generally, frothers are surface active agents that are adsorbed to the air-water interface reducing the surface tension and thereby stabilising the air bubbles. Common frothers are pine oil, alcohols, and certain soaps. The consumption of pine oil ranges between 10 and 100g per tonne of ore.

Finally there are a series of chemical reagents known as regulators or modifiers that are used to enhance or diminish the floatability of minerals thereby permitting the selective flotation of particular minerals. The regulators are subdivided into activators and depressors, pH-regulators and deflocculants.

Activators make a mineral surface more amenable to the adsorption of a collector. They are generally soluble salts which ionise in solution e.g. copper sulphate that activates sphalerite due to its copper ions during flotation with xanthates.

Depressors prevent undesired minerals from floating. They render a mineral surface inactive to a collector by forming a coating on it. Thus the collector cannot connect and the mineral becomes unfloatable.

In selective flotation a strict pH control is essential. PH-regulators such as lime or sulphuric acid provide an optimum pH environment that is needed for flotation of a particular mineral. Generally there is a critical pH above which a mineral will not float.

Dispersing agents or deflocculants are used to control an accumulation of ultra fine particles (“slimes”). These slimes would otherwise adsorb on the surfaces of the minerals to be floated and affect the selectivity of a flotation process. Additionally they would increase the consumption of flotation chemicals by adsorbing them to their large specific surfaces. The amounts of modifiers used per tonne of ore vary as widely as their applications; they range from several grams to a few kilograms.

Flotation is a continuous process. The crude ore which has been ground to an appropriate grain size gets to a conditioner where flotation chemicals are added. The conditioned ore pulp is then pumped to the rougher flotation in which all floatable minerals are recovered. The portion of hydrophobic minerals in the pulp decreases from the first to the last flotation cell of the rougher stage because they are floated in each cell. Theoretically only gangue minerals remain in the pulp which is pumped to the tailings. The relatively impure preconcentrate of the rougher cells then gets to a cleaner flotation in which gangue particles that floated with the ore minerals are depressed to the tailings. The tailings of the cleaner stage can be passed through an additional scavenger flotation in which the few ore particles still remaining in the pulp can be recovered. Until a final concentrate is obtained the pulp has often passed several cleaner and recleaner stages. This is done to produce a concentrate as clean as possible and to minimize losses in ore recovery.

If the ore contains more than one type of valuable mineral we can usually decide between two options. The first is to recover all the valuable components by collective flotation in one single product called bulk concentrate. This can often be done by a simple flotation plant. The second option to recover different minerals from one ore is a selective flotation that produces selective concentrates. Such an operation requires much more sophisticated installations. Usually the valuable minerals are recovered in sequence, one by one. In sulphide flotation the most hydrophobic or the easiest to float are recovered first, followed by the flotation of minerals that are more difficult to float.